| CPC C08B 37/0003 (2013.01) [A23L 27/33 (2016.08); A23L 29/262 (2016.08); A23L 29/30 (2016.08); C08B 37/0057 (2013.01); C08L 5/14 (2013.01); A23V 2002/00 (2013.01); A23V 2200/132 (2013.01); A23V 2200/15 (2013.01); A23V 2200/16 (2013.01); A23V 2200/328 (2013.01); A23V 2200/332 (2013.01); A23V 2250/51088 (2013.01); A23V 2250/61 (2013.01)] | 15 Claims | 
| 
               1. A method for preparing a purified hemicellulose composition comprising: 
            providing a lignocellulosic biomass; 
                combining the lignocellulosic biomass with water; 
                activating the lignocellulosic biomass and water using conditions comprising a temperature and a pressure to form an activated cellulose stream; 
                washing the activated cellulose stream to form a washed activated cellulose stream and a soluble extract, wherein the soluble extract comprises hemicellulose; and 
                purifying the soluble extract to obtain a hemicellulose composition comprising: 
              (a) about 82% to about 92% by dry weight of xylan, wherein said xylan comprises about 70% to about 99% of arabinoxylan; 
                  (b) about 8% to about 9% by dry weight of xylo-oligosaccharide; and 
                  (c) about 4% to about 5% by dry weight of xylose. 
                 |