| CPC C01B 32/20 (2017.08) [C01B 32/21 (2017.08); H01M 4/587 (2013.01); H01M 10/0525 (2013.01); C01P 2004/51 (2013.01); C01P 2006/11 (2013.01); C01P 2006/12 (2013.01); H01M 2004/021 (2013.01); H01M 2004/027 (2013.01)] | 12 Claims |
|
1. A preparation method of modified natural graphite material, the preparation method comprising:
sequentially performing a solidification, an isotropic treatment, a carbonization treatment, and a crushing on a natural graphite as a raw material to obtain the modified natural graphite material,
wherein the natural graphite is prepared by crushing natural flake graphite, and
wherein the natural graphite has all of the following features:
a particle size D50 smaller than 10 μm, and D90/D10<2.5;
a 002 interplanar spacing in a range of 0.336 to 0.360 nm, and 30≤I002/I110≤35;
a saturated tap density greater than or equal to 0.6 g/cc and smaller than1.3 g/cc; and
a specific surface area greater than or equal to 1.0 m2/g and smaller than 10.0 m2/g.
|