CPC A61B 90/18 (2016.02) [A61L 31/041 (2013.01); A61L 31/14 (2013.01); B29C 51/002 (2013.01); C08J 5/18 (2013.01); C08L 67/04 (2013.01); C08L 75/06 (2013.01); B29K 2096/00 (2013.01); B29L 2031/753 (2013.01); C08J 2367/04 (2013.01); C08J 2375/06 (2013.01); C08J 2445/00 (2013.01); C08J 2467/04 (2013.01); C08J 2475/06 (2013.01); C08L 2203/16 (2013.01); C08L 2312/00 (2013.01)] | 18 Claims |
1. A template for a positioning, fixation, mobilization or immobilization device, wherein the template comprises a sheet of an at least partially cross-linked thermoplastic material, wherein the thermoplastic material comprises:
between 3.0 and 95.0 wt. % of a poly-ε-caprolactone polymer, wherein the poly-ε-caprolactone polymer has a number average molecular weight Mn of at least 50.000 g/mole and of maximum 90.000 g/mole, and
at least 5.0 wt. % of at least one second thermoplastic polymer material with a melting temperature of between 40 and 85° C., wherein the at least one second thermoplastic polymer material is one or more of a thermoplastic polyalkenamer or a thermoplastic linear polyurethane based on a poly-ε-caprolactone polyol or a polyester polyol;
wherein the poly-ε-caprolactone polymer and the second thermoplastic polymer material are cross-linked.
|
16. A method for producing an immobilization device, wherein a template according to claim 1 is heated to a temperature between 40 and 85° C., positioned on a body part that needs to be positioned, mobilized or immobilized, shaped to conform to the contours of the body part, and left to cool.
|