CPC C22B 26/12 (2013.01) [C22B 1/02 (2013.01); C22B 3/42 (2013.01)] | 8 Claims |
1. A method for extracting lithium from carbonate clay type lithium ore based on ion exchange, the method comprising the following steps:
(1) Crushing: having lithium ore crushed and finely ground;
(2) Roasting treatment: having crushed ore roasted at a temperature of 450-800° C.;
(3) Iron exchange: adding a solution of ferric iron salt to the ore treated as specified in Step (2), and then conducting iron exchange reaction while stifling;
(4) Filtration and separation: conducting solid-liquid separation immediately after the completion of reaction, the filtrate obtained being a lithium-bearing solution.
|