CPC C08L 23/12 (2013.01) [C08L 23/06 (2013.01); C08L 23/0853 (2013.01); C08L 23/0869 (2013.01); C08L 29/04 (2013.01); C08L 33/08 (2013.01); C08L 51/003 (2013.01); C08L 77/00 (2013.01); C08L 2205/02 (2013.01); C08L 2205/035 (2013.01); C08L 2207/062 (2013.01)] | 17 Claims |
1. A composition comprising:
one or more ethylene polymers;
one or more grafted polyethylenes comprising one or more ethylene-based plastomers and/or grafted high-density polyethylenes;
a vinyl alcohol polymer that is EVOH; and
a polyamide,
wherein a ratio (by weight) of (the vinyl alcohol polymer and the polyamide) to the one or more grafted polyethylenes is from about 89:11 to about 66:34 and
wherein the one or more grafted polyethylenes is an ethylene based plastomer having a melting point of about 25° C. to about 105° C.
|