CPC C04B 33/04 (2013.01) [F01N 13/14 (2013.01); F01N 13/16 (2013.01); B60R 13/0815 (2013.01); B60R 13/0869 (2013.01); F01N 2510/02 (2013.01)] | 4 Claims |
1. A thermal barrier material for use in shielding components of a vehicle from hot surfaces comprising:
35 to 53% of a plurality of clays by weight; and
a remainder comprising one or more of:
magnesium silicate, alumina trihydrate, alumino-borosilicate glass, rock wool, basalt fiber, acrylamide copolymer coagulant, acrylic latex, fatty alcohol alkoxylate, or anionic polyacrylamide, wherein
a sample of the thermal barrier material, when exposed to a temperature of 400° Celsius, produces smoke having a density less than 5 g/cm3 as measured according to the ISO 5659-2:2006(E) standard, and
organic components of the thermal barrier material are limited to between 1.11% and 7.55% by weight.
|