| CPC H10N 30/092 (2023.02) [C08J 3/212 (2013.01); C08J 5/18 (2013.01); C08K 3/22 (2013.01); H10N 30/045 (2023.02); H10N 30/852 (2023.02); C08J 2327/16 (2013.01); C08K 2003/2237 (2013.01); C08K 2201/001 (2013.01); C08K 2201/005 (2013.01)] | 13 Claims |
|
1. A method of producing a lead-free piezoelectric composite, the method comprising:
(a) adding lead-free piezoelectric particles having an average particle size of 200 nm to 1000 nm in a solution comprising a PVDF terpolymer and a solvent having a boiling point ≥80° C. at 0.1 MPa and a solubility in water of ≥0.1 g/g to form a dispersion or suspension;
(b) forming a polymeric matrix having the lead-free piezoelectric particles dispersed therein; and
(c) subjecting the polymeric matrix having the lead-free piezoelectric particles dispersed therein to an electric polarization treatment.
|