| CPC C08F 220/14 (2013.01) [B32B 17/10036 (2013.01); C08F 6/16 (2013.01); C08F 8/44 (2013.01); C08F 210/02 (2013.01); C08F 220/06 (2013.01); C08F 220/1802 (2020.02); C08J 3/14 (2013.01); C08J 5/18 (2013.01)] | 8 Claims |
|
1. A method of manufacturing an ionomer resin, comprising the steps of:
(i) adding a poor solvent to a crude ionomer resin solution comprising a (meth)acrylic acid unit (A), a neutralized (meth)acrylic acid unit (B) and an ethylene unit (C) to allow a granular resin with a peak top particle size of from 50 to 700 μm to be precipitated; and
(ii) washing the precipitated granular resin with a washing solution;
wherein the total amount of the unit (A) and the unit (B) is from 6 to 10 mol % based on the entire monomeric units constituting the crude ionomer resin.
|