| CPC B65D 75/26 (2013.01) [B32B 7/12 (2013.01); B32B 27/08 (2013.01); B32B 27/30 (2013.01); B32B 27/32 (2013.01); B32B 27/34 (2013.01); B32B 2250/02 (2013.01); B32B 2250/03 (2013.01); B32B 2250/05 (2013.01); B32B 2250/24 (2013.01); B32B 2307/31 (2013.01); B32B 2307/406 (2013.01); B32B 2307/7244 (2013.01); B32B 2307/734 (2013.01); B32B 2307/7376 (2023.05); B32B 2439/70 (2013.01)] | 19 Claims | 

| 
               1. A multilayer film comprising: 
            at least one outer layer comprising at least 70% by weight of one or more of an ethylene/alpha-olefin copolymer; 
                and at least one inner layer being an abuse layer comprising a blend of: 
                at least 1% by weight of an anhydride grafted elastomer selected from the group consisting of ethylene propylene diene monomer, ethylene propylene copolymer, styrene-ethylene-butylene-styrene, ethylene/octene copolymer and blends thereof, the anhydride grafted elastomer having a grafting level between 0.1-3.0 wt %; and 
                at least 25% by weight one or more polyamides; 
                wherein at least 5%, 10%, 20%, 30%, 40% or 50% by weight of the multilayer film being of one or more polyamides; the multilayer film having a haze measured according to ASTM D1003 not higher than 20%, and/or a gloss measured according to ASTM D 2457 of at least 90. 
               |