| CPC B01J 20/291 (2013.01) [B01J 20/24 (2013.01); B01J 20/28019 (2013.01); B01J 20/28047 (2013.01); B01J 20/3007 (2013.01); B01J 20/3085 (2013.01); B01J 2220/52 (2013.01)] | 28 Claims |

|
1. A method for manufacturing agar or agarose beads, comprising the steps of:
a) providing a water phase comprising an aqueous solution of agar or agarose at a temperature of 40-100° C.;
b) providing an oil phase comprising a water-immiscible solvent and an emulsifier at a temperature of 40-100° C.;
c) emulsifying said water phase in said oil phase to form a water-in-oil emulsion;
d) cooling said water-in-oil emulsion to a temperature below a gelation temperature of said agar or agarose to form a dispersion of solidified agar or agarose beads; and
e) recovering agar or agarose beads from said dispersion,
wherein said emulsifier comprises a phosphate ester of an alkoxylated fatty alcohol.
|