CPC H01M 10/0562 (2013.01) [C01B 25/14 (2013.01); C01P 2002/30 (2013.01); C01P 2002/72 (2013.01); C01P 2002/86 (2013.01); C01P 2006/40 (2013.01); H01M 2300/0068 (2013.01)] | 18 Claims |
1. A method for producing a sulfide solid electrolyte having an argyrodite crystal structure, the method comprising:
mixing a raw material comprising elemental phosphorus at an integrated power of 0.5 kWh/kg or more; and
heat-treating a precursor obtained in the mixing at a temperature in a range of from 350 to 500° C.
|