CPC C09K 11/7703 (2013.01) [C09K 11/02 (2013.01); C09K 11/77346 (2021.01); C23C 16/40 (2013.01); C23C 16/403 (2013.01); C23C 16/405 (2013.01); C23C 16/407 (2013.01); C23C 16/45529 (2013.01); C23C 16/45553 (2013.01); C23C 18/1254 (2013.01); F21V 9/30 (2018.02); H01L 33/502 (2013.01)] | 19 Claims |
1. A method for providing a luminescent particle with a hybrid coating, the method comprising:
providing a particulate luminescent material having a surface;
forming a primer layer directly on at least a portion of the surface;
performing a first atomic layer deposition process on the particulate luminescent material having the primer layer to deposit a first ALD layer, the first atomic layer deposition process using a metal oxide first precursor selected from a group of metal oxides comprising Al, Zn, Hf, Ta, Zr, Ti, Sn, Nb, Y, Ga, and V;
performing a second atomic layer deposition process to deposit a second ALD layer onto the first ALD layer, the second atomic layer deposition process using a metal oxide second precursor different from the first precursor and selected from a group of metal oxides comprising Al, Zn, Hf, Ta, Zr, Ti, Sn, Nb, Y, Ga, and V; and
performing a main sol-gel coating process to form a main sol-gel coating layer directly onto the second ALD layer, the main sol-gel coating layer having a chemical composition different from the first ALD layer and the second ALD layer.
|