CPC C08L 23/06 (2013.01) [A61F 13/514 (2013.01); A61F 13/51401 (2013.01); A61F 13/51456 (2013.01); A61F 13/51462 (2013.01); A61F 13/51464 (2013.01); A61F 13/551 (2013.01); A61L 15/00 (2013.01); A61L 15/225 (2013.01); A61L 15/42 (2013.01); A61L 15/54 (2013.01); C08J 5/18 (2013.01); C08K 3/22 (2013.01); C08K 3/26 (2013.01); A61F 13/15 (2013.01); C08J 2323/04 (2013.01); C08J 2423/14 (2013.01); C08K 2003/2237 (2013.01); C08K 2003/265 (2013.01)] | 20 Claims |
1. A film comprising:
from about 20 wt. % to about 75 wt. % of a polyolefin component;
from about 5 wt. % to about 35 wt. % of an elastomeric resin; and
from about 20 wt. % to about 45 wt. % of a particle component;
wherein the film has a basis weight of about 5 gsm to about 25 gsm; and
wherein the film has a sound pressure level over a frequency octave range of 2000 Hz-6300 Hz of less than about 43 dB, according to the Sound Pressure Level Test.
|