| CPC G04B 19/12 (2013.01) [A44C 5/02 (2013.01); A44C 27/001 (2013.01); C03B 23/207 (2013.01); C03B 25/02 (2013.01); C03B 29/02 (2013.01); C03C 25/002 (2013.01); G04B 19/042 (2013.01); G04B 37/225 (2013.01); G04D 3/0048 (2013.01)] | 19 Claims |

|
1. A method of manufacturing an exterior part for a timepiece or a piece of jewelry made from Murano glass, said method comprising the following steps:
providing a material formed by glass rods, arranged side by side,
applying a multi-cycle heat treatment to consolidate the material and form a blank,
machining the blank to produce the exterior part, wherein the heat treatment includes a first cycle (a) wherein the material is heated from a first temperature less than or equal to 100 C to a second temperature of between 500 and 600° C. at a heating rate of between 4 and 12° C./min.
|