| CPC C10L 1/08 (2013.01) [C10G 1/02 (2013.01); C10G 1/10 (2013.01); C10G 2300/1003 (2013.01); C10G 2300/202 (2013.01); C10G 2300/301 (2013.01); C10G 2300/304 (2013.01); C10G 2300/308 (2013.01); C10G 2400/04 (2013.01); C10L 2200/0469 (2013.01); C10L 2270/026 (2013.01); C10L 2290/02 (2013.01); C10L 2290/545 (2013.01)] | 16 Claims |

|
1. Composition obtained from the pyrolysis of waste rubber including natural rubber and subsequent separation of the resulting oil, which has:
a flash point of at least 40° C. but no higher than 55° C. determined according to ASTM D93 procedure B,
a boiling point range starting at 100° C. or higher under atmospheric pressure determined according to ASTM D86,
a density at 15° C. of less than 990 kg/m3 determined according to ASTM D4052,
a total acid number (TAN) of up to 12 determined according to ASTM D664,
a styrene content of less than 7000 ppm determined according to gas chromatography, and
an organic halogen (as CI) content of less than 50 mg/kg determined according to IP510, and
which contains biogenic carbon in an amount of at least 15%, as determined according to ASTM D6866 Method B (AMS), and aromatic hydrocarbons with a total aromatic hydrocarbon content of at least 20% m/m, as measured according to IP391.
|