| CPC C08L 77/00 (2013.01) [C08F 210/02 (2013.01)] | 11 Claims |
|
1. A polyamide resin composition consisting of a polyamide resin (I) and an ionomer (II), wherein:
the polyamide resin (I) is a polymer obtained from:
at least one lactam selected from the group consisting of ε-caprolactam, enantholactam, and lauryllactam;
at least one aminocarboxylic acid selected from the group consisting of 6-aminocaproic acid, 7-aminoheptanoic acid, 8-aminooctanoic acid, 9-aminononanoic acid, 11-aminoundecanoic acid, and 12-aminododecanoic acid; or
at least one combination of a diamine and a dicarboxylic acid, wherein:
the diamine is selected from the group consisting of 1,4-butanediamine, 1,5-pentanediamine, 1,6-hexanediamine, 1,5-hexanediamine, 1,9-nonanediamine, 1,11-undecanediamine, 1,12-dodecanediamine, α,ω-diaminopolypropylene glycol, m-phenylenediamine, and p-phenylenediamine, and
the dicarboxylic acid is selected from the group consisting of adipic acid, sebacic acid, dodecanedioic acid, glutaric acid, terephthalic acid, and isophthalic acid; and
the ionomer (II) is an ionomer which satisfies the following requirements:
the ionomer is derived from a copolymer (P) which comprises, as essential constituent units, structural units (A) derived from ethylene and/or an α-olefin having 3 to 20 carbon atoms and structural units (B) derived from a monomer having a carboxyl group and/or a dicarboxylic anhydride group, wherein at least part of the carboxyl group and/or dicarboxylic anhydride group in the copolymer (P) has been converted to a metal-containing carboxylic acid salt containing ions of at least one metal selected from metals belonging to Groups 1, 2, and 12 of the Periodic Table, and wherein the ionomer has a phase angle δ of 50 to 75 degrees at a complex modulus absolute value G* of 0.1 MPa, as measured by a rotational rheometer.
|