| CPC B01D 53/02 (2013.01) [B01D 53/72 (2013.01); B01D 53/8668 (2013.01); B01J 20/0222 (2013.01); B01J 20/28004 (2013.01); B01J 20/28023 (2013.01); B01J 20/3236 (2013.01); B01J 20/3238 (2013.01); B01J 20/324 (2013.01); B01D 2101/02 (2013.01); B01D 2253/102 (2013.01); B01D 2253/25 (2013.01); B01D 2255/2073 (2013.01); B01D 2257/708 (2013.01); B01D 2258/06 (2013.01); B01D 2259/4508 (2013.01); Y02A 50/20 (2018.01)] | 11 Claims |

|
1. A method of forming a material for reacting with volatile organic compounds in a flow of gas, the method comprising:
(a) reacting at least one manganese precursor compound with a reducing agent of the at least one manganese precursor in aqueous phase to form metal oxide nanoparticles;
(b) depositing at least some of the metal oxide nanoparticles in a first porous sorbent having outer surfaces with pores extending internally to define passages, wherein the at least some of the metal oxide nanoparticles deposited in the first porous sorbent are disposed in at least some of the pores and some of the passages: and
(c) applying at least some of the metal oxide nanoparticles to a polymeric fibrous structure.
|