CPC C08L 51/003 (2013.01) [C08F 212/08 (2013.01); C08F 220/44 (2013.01); C08L 25/12 (2013.01); C08L 77/02 (2013.01); C08L 2201/08 (2013.01); C08L 2203/30 (2013.01); C08L 2205/025 (2013.01); C08L 2205/035 (2013.01); C08L 2205/18 (2013.01); C08L 2207/53 (2013.01)] | 15 Claims |
1. A thermoplastic resin composition, comprising:
100 parts by weight of a styrene-based resin;
0.5 to 5 parts by weight of a first polyamide resin having a melting temperature (Tm) of 230° C. or less; and
0.5 to 10 parts by weight of a second polyamide resin having a melting temperature (Tm) of 250° C. or more,
wherein both the first and second polyamide resins have a relative viscosity (1 g per 100 mL of 96% aq. sulfuric acid) of 2.5 or less.
|