CPC C04B 14/22 (2013.01) [B05B 7/20 (2013.01); B22F 3/003 (2013.01); C03B 5/00 (2013.01); C03B 19/10 (2013.01); C04B 7/4453 (2013.01); C04B 14/30 (2013.01); C04B 20/0036 (2013.01); C04B 20/026 (2013.01); C04B 20/04 (2013.01); C04B 35/62665 (2013.01); C09K 8/80 (2013.01); F27B 15/00 (2013.01); F27B 15/10 (2013.01); F27B 15/14 (2013.01); C04B 7/43 (2013.01); C04B 7/44 (2013.01); C04B 2103/0042 (2013.01); C04B 2111/00327 (2013.01); C04B 2235/528 (2013.01); F27B 15/003 (2013.01); Y02P 40/121 (2015.11)] | 20 Claims |
1. A method of reducing CO2 in cement production, comprising the steps of:
forming a cementitious reagent, wherein the cementitious reagent (i) is a non-crystalline solid, (ii) is in the form of a powder, (iii) has a particle distribution with D[3,2] of 20 μm or less, and has less than about 10 wt. % CaO; and
adding the cementitious reagent to a binder.
|