CPC C01G 25/006 (2013.01) [H01M 10/0525 (2013.01); H01M 10/0562 (2013.01); C01P 2002/72 (2013.01); C01P 2002/74 (2013.01); C01P 2002/76 (2013.01); C01P 2002/85 (2013.01); C01P 2004/04 (2013.01); C01P 2004/51 (2013.01); C01P 2004/62 (2013.01); C01P 2004/64 (2013.01); C01P 2006/40 (2013.01); H01M 2300/0077 (2013.01)] | 19 Claims |
1. A method of synthesizing tantalum-doped lithium lanthanum zirconate, the method comprising:
combining a reagent composition with a molten salt composition to yield a salt reaction medium, wherein the reagent composition comprises a lithium component, a lanthanum component, a zirconium component, and a tantalum component;
heating the salt reaction medium to a temperature in a range of 500° C. to 1000° C. to yield a reaction product comprising tantalum-doped lithium lanthanum zirconate,
wherein the salt composition is selected from the group consisting of one of the following mixtures:
a eutectic mixture of potassium chloride and lithium chloride,
lithium hydroxide,
a eutectic mixture of lithium chloride and lithium hydroxide,
a eutectic mixture of lithium bromide and potassium bromide, and
a eutectic mixture of sodium chloride and potassium chloride.
|