CPC H01M 4/525 (2013.01) [H01M 4/131 (2013.01); H01M 4/505 (2013.01); H01M 10/0525 (2013.01); H01M 50/46 (2021.01); H01M 2004/021 (2013.01); H01M 2004/027 (2013.01)] | 5 Claims |
1. An anode material for a secondary battery, comprising:
an oxide mixture obtained by performing a mixing step of at least one of SiO2 and SiO, at least one of SnO and SnO2, and at least one of Fe2O3, Fe3O4 and FeO, wherein an atomic ratio of silicon to tin to iron in the oxide mixture is 4:1:16, 1:1:1, or 4:1:1.
|