CPC C08H 8/00 (2013.01) [C08L 7/02 (2013.01); C08L 9/00 (2013.01); C08L 9/06 (2013.01); C08L 19/003 (2013.01); C08L 53/02 (2013.01); C08L 95/00 (2013.01); C08L 97/005 (2013.01); E01C 5/12 (2013.01); E01C 7/353 (2013.01); C08L 2555/52 (2013.01); C08L 2555/64 (2013.01); C08L 2555/82 (2013.01); C08L 2555/84 (2013.01); C08L 2555/86 (2013.01); Y02A 30/30 (2018.01)] | 38 Claims |
1. A composition comprising bitumen, one or more plasticity modifying agent(s), lignin, and optionally one or more further component(s); wherein said lignin has a Lignin Ion Exchange Capacity (LIEC) of 0.4 mol/kg dry matter (DM) or less.
|