CPC C09J 7/383 (2018.01) [C09J 7/255 (2018.01); C09J 2203/326 (2013.01); C09J 2301/122 (2020.08); C09J 2301/124 (2020.08); C09J 2301/302 (2020.08); C09J 2409/00 (2013.01); C09J 2467/006 (2013.01)] | 16 Claims |
1. A method of producing a cured pressure-sensitive adhesive from a composition comprising:
a) at least one solid acrylonitrile-butadiene rubber,
b) at least one tackifier resin, and
c) optionally at least one liquid acrylonitrile-butadiene rubber,
said method comprising subjecting the composition to electron beam irradiation (EBI) with an acceleration voltage per 1 μm of layer thickness of the composition of 1.8 to 2.38 kV and a total radiation dose of 5 to 50 kGy to obtain the cured pressure-sensitive adhesive.
|