| CPC B05D 7/586 (2013.01) [B05D 1/02 (2013.01); B05D 1/08 (2013.01); B05D 1/18 (2013.01); B05D 1/38 (2013.01); B05D 3/12 (2013.01); B05D 5/00 (2013.01); B05D 7/14 (2013.01); B05D 7/16 (2013.01); B05D 7/22 (2013.01); B05D 7/222 (2013.01); B05D 7/225 (2013.01); B05D 7/26 (2013.01); B05D 7/544 (2013.01); B05D 7/546 (2013.01); B05D 7/584 (2013.01); C08G 77/08 (2013.01); C08G 77/20 (2013.01); C08K 3/22 (2013.01); C08K 5/5425 (2013.01); C09D 5/002 (2013.01); C09D 5/082 (2013.01); C09D 5/084 (2013.01); C09D 7/20 (2018.01); C09D 7/61 (2018.01); C09D 7/62 (2018.01); C09D 7/63 (2018.01); C09D 159/00 (2013.01); C09D 163/04 (2013.01); C09D 183/04 (2013.01); C09D 183/06 (2013.01); C23F 11/18 (2013.01); E21B 33/03 (2013.01); E21B 34/04 (2013.01); E21B 34/06 (2013.01); E21B 41/00 (2013.01); E21B 43/2607 (2020.05); B05D 2202/00 (2013.01); B05D 2202/10 (2013.01); B05D 2254/00 (2013.01); B05D 2350/60 (2013.01); B05D 2401/10 (2013.01); B05D 2504/00 (2013.01); C08G 59/022 (2013.01); C08G 59/063 (2013.01); C08K 3/11 (2018.01); C08K 2003/2241 (2013.01); C08K 2003/2265 (2013.01); C08K 3/36 (2013.01); C08K 5/541 (2013.01); C08K 5/5415 (2013.01); C08K 5/5435 (2013.01); C08K 5/544 (2013.01); C09D 163/00 (2013.01); E21B 17/02 (2013.01); E21B 43/26 (2013.01)] | 19 Claims |

|
1. A method of coating a component, the method comprising:
applying a primer composition to the component;
at least partially curing the primer composition to form a primer layer, such that the primer layer at least partially bonds to the component;
applying a coating composition to the primer layer, the coating composition comprising trifunctional silane, silanol fluid, fillers, and titanium dioxide; and
at least partially curing the coating composition, thereby to form a coating layer and so that the coating layer at least partially bonds to the primer layer to enhance wear resistance of the component, the coating composition comprising T-resin units each of which bonds with one or more of other T-resin units, silanol fluid, fillers, or the titanium dioxide, such that the component exhibits a comparison factor indicative of an increased resistance to wear greater than about 2, the comparison factor being indicative of a first amount of time during which a portion of one or more of: (a) the coating layer or (b) the primer layer, wears to a first depth divided by a second amount of time during which a portion of the component without the one or more of (a) the coating layer or (b) the primer layer wears to a second depth equal to the first depth.
|