| CPC A61L 27/3691 (2013.01) [A61L 2/04 (2013.01); A61L 27/3608 (2013.01); A61L 27/3683 (2013.01); A61L 27/3687 (2013.01); A61L 27/3847 (2013.01); A61P 19/08 (2018.01); A61L 2430/12 (2013.01)] | 9 Claims |
|
1. A method for making a non-resorbable bone allograft, the method comprising:
excising a bone allograft from a human donor's body;
freeze-drying the bone allograft;
thermal processing a first set of the freeze-dried bone allograft, wherein the first set of the freeze-dried bone allograft is mineralized, and wherein the thermal processing is performed:
(i) at a temperature about 1,200 degrees Celsius for about one hour;
(ii) at a temperature about 900 degrees Celsius for about four hours; or
(iii) at a temperature about 300 degrees Celsius for about twelve hours, thus forming a non-resorbable, mineralized first set of bone allograft; and
preserving and sterilizing the non-resorbable, mineralized first set of bone allograft.
|