| CPC H01M 10/0565 (2013.01) [C01B 32/194 (2017.08); C01B 32/198 (2017.08); C01B 32/23 (2017.08); H01M 10/0525 (2013.01); H01M 10/0585 (2013.01); H01M 50/119 (2021.01); H01M 50/121 (2021.01); H01M 50/129 (2021.01); C01B 2204/22 (2013.01); H01M 2300/0082 (2013.01); Y02E 60/10 (2013.01); Y02P 70/50 (2015.11); Y02T 10/70 (2013.01)] | 6 Claims |

|
1. A method for forming a graphene compound, comprising the steps of:
stirring graphene oxide and a base under a nitrogen stream to form a first mixture;
cooling the first mixture after the stirring step; and
adding a silylating agent to the first mixture after the cooling, to form a second mixture,
wherein the silylating agent further comprises a chain group comprising two or more ether bonds,
wherein the chain group has a structure terminated with an alkoxyalkyl group, and
wherein the base is any one of butylamine, pentylamine, hexylamine, diethylamine, dipropylamine, dibutylamine, triethylamine, tripropylamine and pyridine.
|