CPC C08J 7/123 (2013.01) [C08J 5/124 (2013.01); H05K 1/034 (2013.01); C08J 2327/18 (2013.01)] | 14 Claims |
1. A fluorine resin surface modification method comprising the steps of:
irradiating an organic compound containing an oxygen atom with ultraviolet light having at least an intensity in a wavelength range of 205 nm or less, while the organic compound containing the oxygen atom is continuously supplied in gaseous form, to generate a radical; and
bringing the radical into contact with a surface of a fluorine resin to form a hydrophilized layer on the surface, wherein the fluorine resin, after the process of forming the hydrophilized layer on the surface, has the surface which has a peak intensity of carbon atoms and a peak intensity of oxygen atoms that are higher than a peak intensity of fluorine atoms in a photoelectron spectrum by XPS survey analysis.
|