US 12,215,059 B2
Activation of ground granulated blast furnace slag
Lissa Dupouy, Issy-les-Moulineaux (FR); Maxime Liard, Zürich (CH); Lolita Hauguel, Zürich (CH); and Didier Lootens, Küsnacht (CH)
Assigned to SIKA TECHNOLOGY AG, Baar (CH)
Appl. No. 17/281,153
Filed by SIKA TECHNOLOGY AG, Baar (CH)
PCT Filed Oct. 1, 2019, PCT No. PCT/EP2019/076513
§ 371(c)(1), (2) Date Mar. 29, 2021,
PCT Pub. No. WO2020/070093, PCT Pub. Date Apr. 9, 2020.
Claims priority of application No. 18198197 (EP), filed on Oct. 2, 2018.
Prior Publication US 2021/0340065 A1, Nov. 4, 2021
Int. Cl. C04B 22/06 (2006.01); C04B 7/02 (2006.01); C04B 22/10 (2006.01); C04B 22/14 (2006.01); C04B 28/08 (2006.01); C04B 103/12 (2006.01); C04B 103/14 (2006.01); C04B 103/32 (2006.01)
CPC C04B 28/08 (2013.01) [C04B 7/02 (2013.01); C04B 22/064 (2013.01); C04B 22/10 (2013.01); C04B 22/106 (2013.01); C04B 22/143 (2013.01); C04B 22/147 (2013.01); C04B 2103/12 (2013.01); C04B 2103/14 (2013.01); C04B 2103/32 (2013.01)] 9 Claims
 
1. A mineral binder composition comprising:
a mineral binder comprising 36-65 weight-% of slag and 35-64 weight-% of Portland cement, based on the weight of the mineral binder,
an activator for the hydration of the slag comprising calcium hydroxide and
a co-activator comprising at least one salt selected from the group consisting of lithium carbonate, lithium sulfate and sodium carbonate,
wherein the activator is present in an amount in a range of 0.5-3.0 weight-% based on the weight of the mineral binder,
wherein the co-activator is present in an amount in a range of 0.16-0.8 weight-% based on the weight of the mineral binder, and
wherein a weight-ratio of activator to co-activator is 10:1 to 1.1:1.