| CPC B02C 19/0056 (2013.01) [B09B 3/50 (2022.01); C08L 95/00 (2013.01); C09D 195/00 (2013.01); C08L 2555/34 (2013.01)] | 20 Claims | 

| 
               1. A method comprising: 
            obtaining an asphalt shingle waste; 
                feeding the asphalt shingle waste at a first temperature to an inlet of a microwave dryer; 
                exposing the asphalt shingle waste to microwaves emitted by the microwave dryer; 
                discharging the asphalt shingle waste at a second temperature at an outlet of the microwave dryer, 
                wherein the second temperature is a temperature of 140° F. or less; 
                  wherein a moisture content of the asphalt shingle waste at the outlet of the microwave dryer is less than a moisture content of the asphalt shingle waste at the inlet of the microwave dryer; and 
                processing the asphalt shingle waste. 
               |