CPC D21H 23/56 (2013.01) [D21H 19/32 (2013.01); D21H 19/54 (2013.01); D21H 21/16 (2013.01); D21H 21/20 (2013.01); D21H 21/24 (2013.01)] | 7 Claims |
1. A method of treating paper, comprising:
applying a composition onto a paper press roll to form a coated paper press roll, the composition comprising a strength agent, a sizing agent, and a surfactant; and
contacting paper with the coated paper press roll to form a treated paper,
wherein the treated paper has a Cobb value equal to or less than a Cobb value of paper treated with the strength agent and the sizing agent but not with the surfactant;
wherein the strength agent is about 1 wt % to about 10 wt % of the composition;
wherein the surfactant is about 0.005 wt % to about 0.5 wt % of the composition; and
wherein the surfactant is an alkoxylated ethylenediamine, or wherein the surfactant comprises formula I:
![]() wherein
n is an integer ranging from 0 to 100;
m is an integer ranging from 0 to 100;
x is an integer ranging from 1 to 3;
y is an integer ranging from 0 to 5; and
R1 is hydrogen, halogen, C1-10 alkyl, phenyl, or cycloalkyl.
|