CPC D04H 3/011 (2013.01) [D04H 3/073 (2013.01); A47G 27/02 (2013.01); D10B 2331/04 (2013.01); D10B 2503/041 (2013.01)] | 8 Claims |
1. A spunbonded nonwoven fabric comprising
a fiber web of mixed filament yarns of a first filament prepared from a polyester and a recycled polyester each having a melting point of 255° C. or more; and a second filament prepared from a copolyester having a lower melting point than that of the first filament by 30° C. or more,
wherein the first filament is a filament having a hollow fiber cross-section having a hollow ratio of 10 to 20%,
wherein a raw material of the recycled polyester has an average number of foreign matters with a size of 1.0 to 10.0 μm, of 10 or less, and
wherein the spunbonded nonwoven fabric has tensile strength of 20 kgf/5 cm or more and tensile elongation of 20% or more as measured according to the KS K 0521 test method, and is used as a base fabric for tile carpets.
|