CPC C08L 9/06 (2013.01) [B60C 1/0016 (2013.01); C08L 2205/025 (2013.01); C08L 2205/035 (2013.01)] | 18 Claims |
1. A rubber composition comprising:
70 phr to 95 phr of styrene butadiene rubber comprising at least 5 phr of a first styrene butadiene rubber having a glass transition temperature determined as a peak midpoint by differential scanning calorimeter (DSC) at a temperature rate of increase of 10° C. per minute according to ASTM D3418 within a range of −49° C. to −15° C. and at least 45 phr of a second styrene butadiene rubber having a glass transition temperature within a range of −50° C. to −75° C., wherein the rubber composition comprises more of the second styrene butadiene rubber than of the first styrene butadiene rubber;
5 phr to 30 phr of at least one member selected from the group consisting of natural rubber and synthetic polyisoprene rubber;
more than 150 but less than 200 phr of filler including both silica and coupling agent; and
at least 55 phr of at least one hydrocarbon resin comprising at least one terpene resin which has a glass transition temperature of at least 30° C.; and,
optionally 1 phr to 4 phr of oil.
|