CPC C08L 27/24 (2013.01) | 7 Claims |
1. A chlorinated polyvinyl chloride resin having an average of a ratio (A/B) of a peak intensity A observed in a range of 660 to 700 cm−1 to a peak intensity B observed in a range of 600 to 650 cm−1 of 0.50 to 2.00 in Raman imaging measurement by Raman spectroscopy, and having a standard deviation of the ratio (A/B) of the peak intensity A to the peak intensity B of 0.100 to 0.200 in Raman measurement by Raman spectroscopy,
wherein the chlorinated polyvinyl chloride resin contains units (a) to (c) represented by the following formulas (a) to (c), and a proportion of the structural unit (a) is 5.0 mol % or higher, a proportion of the structural unit (b) is 40.0 mol % or lower, and a proportion of the structural unit (c) is 55.0 mol % or lower, relative to a total number of moles of the structural units (a), (b), and (c)
|