CPC B32B 27/20 (2013.01) [B29C 48/022 (2019.02); B29C 48/08 (2019.02); B29C 48/21 (2019.02); B29C 48/28 (2019.02); B29C 48/40 (2019.02); B29D 7/01 (2013.01); B32B 27/36 (2013.01); B32B 37/153 (2013.01); B29K 2067/00 (2013.01); B29K 2105/0005 (2013.01); B29K 2995/0026 (2013.01); B32B 37/06 (2013.01); B32B 2250/02 (2013.01); B32B 2255/10 (2013.01); B32B 2264/102 (2013.01); B32B 2307/744 (2013.01); B32B 2367/00 (2013.01); B32B 2377/00 (2013.01); B32B 2439/70 (2013.01)] | 9 Claims |
1. A method of making a laminate comprising the steps of:
forming a heat seal resin composition by mixing a copolyester resin component, an antifog additive, and an anti-block and slip additive in the absence of a solvent, wherein the copolyester resin comprises a blend of a semi-crystalline copolyester resin and an amorphous copolyester resin;
applying the heat seal resin composition to a film-forming compound, such as polyester, or a film, such as a polyester film, to form the laminate, wherein no solvent is added to the heat seal resin composition before or during the applying step.
|