CPC C09D 11/10 (2013.01) [B41M 1/10 (2013.01); C08K 3/22 (2013.01); C08K 3/30 (2013.01); C08K 5/0025 (2013.01); C08K 5/0041 (2013.01); C08K 5/01 (2013.01); C08L 33/08 (2013.01); C09D 11/037 (2013.01); C08K 2003/2241 (2013.01); C08K 2003/3036 (2013.01); C08L 2201/52 (2013.01); C08L 2205/20 (2013.01)] | 15 Claims |
1. A method of improving die cutting blade durability, comprising the steps of:
providing an opaque ink comprising water as a volatile component and an opacifying component, wherein the opacifying component comprises 1.0 wt % to 100 wt % hollow sphere resin particles and 0 wt % to 90 wt % of a colorant that is one or more abrasive white pigments, on a solid weight basis of the opacifying component;
printing the ink on a substrate; and
cutting the printed substrate with a die cutting blade;
wherein the durability of the die cutting blade is improved, relative to the durability of a die cutting blade used to cut a substrate printed with an ink comprising an opacifying component containing 100 wt % of a colorant that is abrasive white pigment, on a solid weight basis of the opacifying component.
|