CPC C04B 35/80 (2013.01) [C04B 35/6269 (2013.01); C04B 35/62871 (2013.01); C04B 35/62886 (2013.01); C04B 35/632 (2013.01); C04B 35/64 (2013.01); C08G 77/62 (2013.01); C08G 79/08 (2013.01); C04B 2235/3856 (2013.01); C04B 2235/3873 (2013.01); C04B 2235/483 (2013.01); C04B 2235/486 (2013.01); C04B 2235/5252 (2013.01); C04B 2235/616 (2013.01); C04B 2235/721 (2013.01)] | 11 Claims |
1. A method for manufacturing a part made of composite material comprising:
forming a ceramic matrix phase in pores of a fibrous preform by pyrolysis of a cross-linked copolymer ceramic precursor, said cross-linked copolymer comprising a first precursor macromolecular chain of a first ceramic having free carbon, and a second precursor macromolecular chain of a second ceramic having free silicon, the first macromolecular chain being bonded to the second macromolecular chain by cross-linking bridges comprising a bonding structure of formula *1—X—*2; in this formula, X designates boron or aluminium, -*1 designates the bond to the first macromolecular chain and -*2 the bond to the second macromolecular chain.
|