CPC C08L 23/16 (2013.01) [C08F 4/6592 (2013.01); C08F 4/65912 (2013.01); C08F 210/02 (2013.01); C08F 210/06 (2013.01); C08F 210/08 (2013.01); C08F 210/18 (2013.01); C08F 236/20 (2013.01); C08K 3/04 (2013.01); C08K 3/22 (2013.01); C08K 5/0025 (2013.01); C08K 5/098 (2013.01); C08L 91/00 (2013.01); F16H 7/023 (2013.01); C08K 2003/2296 (2013.01); C08L 2205/035 (2013.01); C08L 2310/00 (2013.01)] | 22 Claims |
1. An elastomeric composition comprising:
from 5 to 40 parts by weight per hundred parts by weight rubber (phr) of a propylene-α-olefin-diene (PEDM) terpolymer comprising 75 to 95 wt % propylene, 5 to 20 wt % α-olefin, and 0.5 to 5 wt % diene, said wt % based on the weight of the PEDM terpolymer, wherein the PEDM terpolymer has an Hf less than half 1 J/g; and
from 60 to 95 phr of an ethylene-based copolymer comprising ethylene, one or more C3 to C12 α-olefins, and, optionally, one or more dienes; wherein an ethylene-based based copolymer comprises 40 to 95 wt % ethylene, 0 to 10 wt % of one or more dienes, and a C3 to C12 α-olefin, said wt %s based on a total weight of the ethylene-based copolymer.
|