Int. Cl. C04B 28/06 (2006.01); C04B 14/06 (2006.01); C04B 14/28 (2006.01); C04B 24/26 (2006.01); C04B 24/38 (2006.01); C04B 41/00 (2006.01); C04B 41/50 (2006.01); C04B 41/65 (2006.01); E04H 13/00 (2006.01); B28B 1/14 (2006.01); C04B 103/32 (2006.01); C04B 103/50 (2006.01); C04B 103/60 (2006.01); C04B 111/54 (2006.01)
CPC C04B 28/06 (2013.01) [C04B 14/06 (2013.01); C04B 14/068 (2013.01); C04B 14/28 (2013.01); C04B 24/2641 (2013.01); C04B 24/38 (2013.01); C04B 24/383 (2013.01); C04B 41/009 (2013.01); C04B 41/50 (2013.01); C04B 41/65 (2013.01); E04H 13/00 (2013.01); B28B 1/14 (2013.01); C04B 2103/32 (2013.01); C04B 2103/50 (2013.01); C04B 2103/60 (2013.01); C04B 2111/545 (2013.01)] 17 Claims
 
1. A polymer cement-granite composite tomb box, comprising: a layered structure;
wherein the layered structure is formed by compounding one layer of a granite slab or two layers of granite slabs and one layer of a polymer cement;
wherein the polymer cement consists of 20-35 parts by weight of a cement, 25-45 parts by weight of a fine aggregate, 25-55 parts by weight of a coarse aggregate, 0.01-0.5 part by weight of a superplasticizer, 1-6 parts by weight of a polymer, 0.001-0.005 part by weight of a retarder, 0.01-0.1 part by weight of an anti-cracking strengthening agent, 0.01-10 part by weight of a stabilizer, and 0.001-0.5 part by weight of an antifoaming agent and a surface of the polymer cement is coated with a marble coating.