CPC B32B 27/327 (2013.01) [B29C 65/18 (2013.01); B29C 66/1122 (2013.01); B29C 66/71 (2013.01); B29C 66/723 (2013.01); B29C 66/7313 (2013.01); B29C 66/73921 (2013.01); B32B 7/08 (2013.01); B32B 27/08 (2013.01); B32B 2250/05 (2013.01); B32B 2250/246 (2013.01); B32B 2307/72 (2013.01); B32B 2439/40 (2013.01); B32B 2439/70 (2013.01); C08F 2/01 (2013.01)] | 17 Claims |
1. A stand up pouch comprising:
a first layer and a second layer of a multilayer film wherein the first layer is heat bonded to the second layer, and the multilayer film comprises:
a first skin layer consisting of from 85 to 100 weight % of a high density polyethylene having a density of from 0.95 to 0.97 g/cc and a melt index, I2, of from 0.5 to 10 g/10 minutes;
a second skin layer consisting of from 85 to 100 weight % of a first linear low density interpolymer having a molecular weight distribution Mw/Mn of from 2.5 to 4.0, a density of from 0.90 to 0.92 g/cc, a melt index, I2, of from 0.3 to 3 g/10 minutes and a Dilution Index, Yd, of greater than 0°; and
a core comprising medium density polyethylene having a density of from 0.930 to 0.95 g/cc;
with the proviso that the stand-up pouch comprises at least 90% by weight polyethylene; and
wherein, the first layer of multilayer film is heat bonded to the second layer of multilayer film such that the second skin layer of the first layer is in contact with the second skin layer of the second layer.
|