CPC C08J 3/092 (2013.01) [C08J 3/005 (2013.01); C08J 2353/02 (2013.01); C08J 2445/02 (2013.01); C08J 2471/12 (2013.01)] | 32 Claims |
1. A thermoplastic gel prepared from a composition comprising:
1 wt % to 25 wt % of a styrene triblock copolymer;
1 wt % to 16 wt % of a styrene diblock copolymer;
60 wt % to 90 wt % of an oil extender; and
0.25 wt % to 15 wt % of an additive, wherein the additive is selected from the group consisting of poly(2,6-dimethyl-1,4-phenylene oxide), poly(alpha-methylstyrene), and combinations thereof,
wherein the additive has a Tg from about 95° C. to about 200° C., and wherein the gel has a compression set below 25% at about 70° C.
|