Preparation method of anode slurry and battery
Zhongxun Xiu, Changzhou (CN); Taotao Shen, Changzhou (CN); and Junli Tong, Luoyang (CN)
Assigned to CALB Technology Co., Ltd., Jiangsu (CN); and CALB Co., Ltd., Jiangsu (CN)
Filed by CALB Technology Co., Ltd., Jiangsu (CN); and CALB Co., Ltd., Jiangsu (CN)
Filed on Jul. 22, 2021, as Appl. No. 17/382,347.
Claims priority of application No. 202110570443.4 (CN), filed on May 25, 2021.
Prior Publication US 2022/0384814 A1, Dec. 1, 2022
Int. Cl. H01M 4/62 (2006.01); H01M 4/02 (2006.01); H01M 4/587 (2010.01)
CPC H01M 4/622 (2013.01) [H01M 4/587 (2013.01); H01M 4/624 (2013.01); H01M 2004/027 (2013.01)] 5 Claims
OG exemplary drawing
 
1. A preparation method of an anode slurry, comprising:
S12, mixing materials containing a plasticizer, an additive, and a solvent to form a premixed slurry B;
S13, mixing the materials containing the premixed slurry B, an anode active material, and a conductive agent to form a premixed slurry A; and
S2, mixing a styrene-butadiene rubber emulsion with the premixed slurry A;
wherein the plasticizer comprises a first functional group, the first functional group comprises at least one of a hydroxyl group, a carbonate group, and a ketone group, the additive comprises a second functional group, and the second functional group comprises at least one of a carboxyl group, a nitrile group, and an amide group.