CPC B01J 20/043 (2013.01) [B01J 20/3204 (2013.01); B01J 20/3236 (2013.01); C01B 32/60 (2017.08); C01F 5/24 (2013.01); C01F 11/182 (2013.01); C04B 14/26 (2013.01); C04B 18/06 (2013.01); B01D 53/62 (2013.01); B01D 53/82 (2013.01); B01D 2251/304 (2013.01); B01D 2251/306 (2013.01); B01D 2251/402 (2013.01); B01D 2251/404 (2013.01); B01D 2251/606 (2013.01); B01D 2257/504 (2013.01); B01D 2259/4591 (2013.01); B01J 4/00 (2013.01); B01J 19/06 (2013.01); B01J 19/24 (2013.01); Y02C 20/40 (2020.08)] | 16 Claims |
1. A method of producing a solid CO2 sequestering carbonate material, the method comprising:
introducing a divalent cation source into a flowing aqueous bicarbonate and/or carbonate containing liquid under conditions sufficient such that a non-slurry solid phase CO2 sequestering carbonate material is produced in the flowing aqueous bicarbonate and/or carbonate containing liquid.
|