CPC C01G 35/006 (2013.01) [C01G 41/006 (2013.01); C04B 35/495 (2013.01); H01B 3/12 (2013.01); C04B 2235/3206 (2013.01); C04B 2235/3215 (2013.01); C04B 2235/3255 (2013.01); C04B 2235/326 (2013.01); C04B 2235/768 (2013.01); C04B 2235/77 (2013.01); C04B 2235/80 (2013.01)] | 20 Claims |
1. A method of making a high Q material comprising:
providing Ba3NiTa2O9; and