CPC C01B 32/354 (2017.08) [C01B 32/05 (2017.08); C01B 32/21 (2017.08); C01B 32/348 (2017.08); C08L 33/20 (2013.01); C01P 2006/12 (2013.01); C01P 2006/14 (2013.01); C01P 2006/17 (2013.01)] | 19 Claims |
1. A method for preparation of mesoporous nitrogen-doped carbon comprising forming a composition by solubilizing a nitrogen-containing polymer in an aqueous solution of ZnCl2 and drying the aqueous solution, the method further comprising heating the composition after drying to a temperature to carbonize the nitrogen-containing polymer to form the mesoporous nitrogen-doped carbon.
|