CPC H01G 11/32 (2013.01) [H01G 11/62 (2013.01); H01G 11/64 (2013.01); H01G 11/86 (2013.01)] | 14 Claims |
1. A method for making a nanocomposite electrode, comprising:
mixing at least one binding compound, at least one conductive additive, and at least one electrolyte to form a slurry;
mixing nitrogen-doped molybdenum carbide nanosheets with the slurry to form a synthesis mixture;
coating the synthesis mixture onto a surface of an electrode substrate; and
drying the nanocomposite electrode at a temperature less than 100° C. to form the nanocomposite electrode;
wherein the nanocomposite electrode comprises:
the electrode substrate;
the nitrogen-doped molybdenum carbide nanosheets;
the at least one electrolyte;
the at least one binding compound; and
the at least one conductive additive;
wherein the electrolyte at least partially penetrates pores of the nitrogen-doped molybdenum carbide nanosheets; and
wherein the nitrogen-doped molybdenum carbide nanosheets are an outer layer of the nanocomposite electrode.
|